After cured resin in the carbon fiber can customize it with print vinyl?
Can I go back to put another layer of resin over the vinyl for you to have protection and without gaining air bubbles?
Best Regards,
Jorge Ferreira
By Warren (Staff)
-
4/2/2015 4:03:43 PM
Clear coating is best in this situation. However we always recommend testing on a bit of scrap first as sometimes the vinyl curls or if its been printed, the inks run.