Hi 

i plan on making a Roll Wrapped carbon fiber tube of 90mm ID and 97mm OD.I was planing on using 12k 400gsm plain weave Carbon fiber material for the same but i am concerned that the cloth will not conform well to the mandrel at the time of wrapping.I plan to vacuum bag after wrapping it manually .

So will 12k 400gsm plain weave cloth work or do i need to change the weave/cloth?

Please help
Edited 11 Years Ago by M Hathiyari
Reply
VVS
VVS
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
I'm probably following the same road you've been down.

Restoring an old race bike and foolishly decide to replace glass with carbon.

The important dimension with the tube was the inside so that o could reuse the ti end caps.

Back to the initial post and there will be different issues with the much thicker wall thickness, should be much easier to remove due to the extra mass of the tube.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
M Hathiyari - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
M Hathiyari - 11 Years Ago
ChrisR - 11 Years Ago
VVS - 11 Years Ago
mep12rid - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
M Hathiyari - 11 Years Ago
VVS - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search