Determine which fabric to chose while roll wrapping a 90mm rod


Author
Message
M Hathiyari
M Hathiyari
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 4, Visits: 29
Hi 

i plan on making a Roll Wrapped carbon fiber tube of 90mm ID and 97mm OD.I was planing on using 12k 400gsm plain weave Carbon fiber material for the same but i am concerned that the cloth will not conform well to the mandrel at the time of wrapping.I plan to vacuum bag after wrapping it manually .

So will 12k 400gsm plain weave cloth work or do i need to change the weave/cloth?

Please help
Edited 11 Years Ago by M Hathiyari
Reply
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
@VVS

With your method of using heatshrink tubing you start off wrapping a relatively cold Aluminium mandrel. then heating the entire thing to a high temperature (to activate the heatshrink tubing/tape you will be well above 100 degrees)

The tubing shrinks, and the Alu mandrel expands (more than you would think)!, and since both shrink tape and especially the tubing is elastic, it will keep a tight wrap on the CF/resin as the mandrel cools down, keeping the CF tube tightly pressed against the mandrel. Which is all good, from a curing point of view, but the heat also deteriorates the thin layers of wax or chem release, and may distort the combination of release film and wax/release to the point where it locks the composite into any microscopic imperfection in the mandrel.

It is quite possible that cooling the mandrel will not shrink it enough to have any effect on the CF tube, a 1 mm tube will still be a bit elastic on the circumference, and so it just stays attached to the mandrel.

As I said, I think the vaseline works because it forms a thicker layer, and in effect also "lubricates" the inner surface of the release-film, making it possible to slide the tube off the mandrel, wax or chem-lease does not have that "lubricating" effect.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
M Hathiyari - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
M Hathiyari - 11 Years Ago
ChrisR - 11 Years Ago
VVS - 11 Years Ago
mep12rid - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
M Hathiyari - 11 Years Ago
VVS - 11 Years Ago