I noticed you're from NZ, We are from Australia, and funnily enough, we are having the EXACT same problems.
We did notice when setting it up the vacuum infusion during the day as opposed to later at night when it was colder, we did have a much better finish.
We also found that infusing at a constant and reasonably quick rate gave us the best results. Keep in mind this was for small items. We did try slowing it down however that caused a s*** load of air voids like in the edge of your product.
Will definitely try clamping off the vacuum line first and then the feed line as i think we've been doing it the opposite way.
|