Infusing a laminate made up of Unidirectional Tow AND twill fabric


Infusing a laminate made up of Unidirectional Tow AND twill fabric
Author
Message
baja_patient
baja_patient
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Hi Guys,

Quick question, I have read several times that it is difficult/impossible to infusive unidirectional carbon, especially in a thicker laminate.

I wanted to create a landing gear for a model plane, and I woul make it approx 3mm thick, using BOTH carbon spread tow (about 25mm wide) and a couple of layers of a fabric each side (either a 200gsm canvas, 2x2 twill, or satin harness weave).

Would it be possible to do this in infusion with the fabric on both sides of the "uni directional core"? Or would the resin not flow and/or permeate?

Below is a picture to show a similar finished product, one is pure uni and one is a mix (like i am planning).

I assume they are done in wetlay. Which I suppose would also be possible, but a bit heavier and less stiff.

http://www.talkcomposites.com/Uploads/Images/dc8490e1-7b94-4759-b233-4110.png

Cheers People!
Reply
baja_patient
baja_patient
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Thanks guys, I may try both methods, maybe start out with a wet lay. (by wet lay I did mean vacuum bagging it afterwards).

So Mould - Laminate - Perforated release film - breather - vac bag?

Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search