Hi I want to make a mould of my bonnet which is 145cm x 115cm which size unimold kit would I need regular or the larger one

Thanks Paul 
Reply
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
The small Uni-Mould kit is for 0.7 Sq Metres. As your bonnet is 1.6 Sq Metres You will need 3 of these. For £30 more, the larger kit will give you twice as much as you need. If you are following the Easy Composites video and making the inner skin as well this should be ideal.
(Yes, Moulds are expensive!)

Brian.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search