The small Uni-Mould kit is for 0.7 Sq Metres. As your bonnet is 1.6 Sq Metres You will need 3 of these. For £30 more, the larger kit will give you twice as much as you need. If you are following the Easy Composites video and making the inner skin as well this should be ideal. (Yes, Moulds are expensive!)