Early troubleshooting with air voids, pin holes and dry spots


Author
Message
JakeMiddleton
JakeMiddleton
Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)
Group: Forum Members
Posts: 1, Visits: 2
http://www.talkcomposites.com/Uploads/Images/8ffb4164-077b-4160-bf85-a111.JPG http://www.talkcomposites.com/Uploads/Images/098991c6-92ee-4aef-a8f1-f01d.JPGhttp://www.talkcomposites.com/Uploads/Images/4bbed813-1dee-46e6-a15b-b943.JPG Hello I am embarking on a project to improve the concertina (a small accordion traditionally 6 sided) ergonomically, part of this is done by reducing the weight with carbon fibre components. The two components I am making are the ends and here is a picture of one of these ends, the components  are quite small at 200mmx120mm.  I am using resin infusion and the problems I am running into are dry spots, small bubbles and large voids (see images). I am using the large epoxy mould making kit and I have included an image of my mould. I have tried to push the bag around into every contour but still suffer from these problems. What would you guys advise?
Reply
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
There could be numerous issues with the process. But one thing ive noticed is that you have a very small radius in the centre to the 90degree walls. You need to ensure that the material gets right into the corner and doesnt bridge. You can use multiple plys in that area and when bagging use a dibber to prod the material into place prioe and post infusion to make sure there is material and not just resin in the corner