Need help with prepeg technology
Need help with prepeg technology
Post Reply
Like
2
Need help with prepeg technology
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ZairMirza
ZairMirza
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 19
Hello.
I'm Zair from Armenia , i newbie in carboan foaming and i need help pls.
For first i present as i make carbon part
1) I make aluminium mold
2) I put carbon prepreg into the mould ( do not have photo)
3) I make special vacuum thermopocket
4) Make vacuum with my compressor and put it into oven. 30 minutes 100C and 2 Hours 140C
5) When it finished i have some problem with parts, check photos
The edges are not glued. I think that problem is that the vacuum is not enough effort to flatten the material inside the mold.
I think autoclave can resolve it problem, but it so expensive for me
Pls how i can resolve it?
Reply
Like
2
Reply
Fasta
Fasta
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
It looks like your one bag technique should work ok as it then folds back over the whole mould same as having two bags taped together.
I think maybe you should consider putting some carbon in each mould half separate and then vacuum bag this first with just 70 deg for 30 minutes.
Then add more material to make the carbon join properly as you close the moulds with your bag as before. Then cook.
Fastacraft Facebook page
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Need help with prepeg technology
ZairMirza
-
10 Years Ago
I cant tell from your photos of the bag but are you using two bags? An internal bladder and an...
scottracing
-
10 Years Ago
[b]scottracing (11/01/2015)[/b][hr]I cant tell from your photos of the bag but are you using two...
ZairMirza
-
10 Years Ago
In future i want make this part What better and cheap - make 1 detail or two halves and...
ZairMirza
-
10 Years Ago
Just a note on designing CF parts ... You will get much stronger parts by having a proper "radius"...
Dravis
-
10 Years Ago
Big thx for your answer. 1) Yes, we use one bag. how we can use two bags? You need to run one bag...
scottracing
-
10 Years Ago
It looks like your one bag technique should work ok as it then folds back over the whole mould same...
Fasta
-
10 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search