Hey guys,

New to the composite industry, and have just successfully completed our first mould (Phew).
Was just wondering what is the best way to remove excess filleting wax that is left over on the mould? Tried scraping it off, and using just a regular microfibre cloth, or my finger. Majority of it has been removed however there are still some areas that have it smeared.

Thanks in advance,
JD
carbonfibreworks
carbonfibreworks
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi JD
Easy composites mould cleaner is ideal for removing the fillet wax.
Regards Chris
Carbon fibre works LTD

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 11 Years Ago by carbonfibreworks
Matthieu Libeert
Matthieu Libeert
Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
or thinner Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




JustJDee
JustJDee
Supreme Being (137 reputation)Supreme Being (137 reputation)Supreme Being (137 reputation)Supreme Being (137 reputation)Supreme Being (137 reputation)Supreme Being (137 reputation)Supreme Being (137 reputation)Supreme Being (137 reputation)Supreme Being (137 reputation)
Group: Forum Members
Posts: 13, Visits: 153
Ahhh great, too easy! I'm assuming thinner won't affect or damage the tooling gel coat?

Thanks guys,
JD
Matthieu Libeert
Matthieu Libeert
Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)Supreme Being (8.2K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
better test it on a small part of the mould first, didnt ever affect anything on my gelcoat Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




JaseYPK
JaseYPK
Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)
Group: Forum Members
Posts: 7, Visits: 36
Car brake cleaner removes everything from anything. Spray on, wipe off! (Again test first)
kidpaint
kidpaint
Supreme Being (930 reputation)Supreme Being (930 reputation)Supreme Being (930 reputation)Supreme Being (930 reputation)Supreme Being (930 reputation)Supreme Being (930 reputation)Supreme Being (930 reputation)Supreme Being (930 reputation)Supreme Being (930 reputation)
Group: Forum Members
Posts: 99, Visits: 676
Brake cleaner is basically Acetone. Ive noticed acetone can sometimes leave a smug or kinda greasy looking streak where you wiped it so i always go back with a clean dry towel and remove that streak. Ive also used compressed air to blow it out, or depending on how many little spots there are. Like suggest above, mold cleaner. 