Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I would disagree with building it to the same weight as the metal part it is replacing, though to some extent that does depend on the mechanical strength required. The general rule of thumb is to build it to the same THICKNESS as the metal part it is replacing. So if the original part is a 2mm thick steel tube, then a 2mm thick carbon tube should be ideal.
|