I was wondering if there is a way to create a resin to drop on a tissue to obtain a material whose appearance is similar to industrial prepreg, that is to say a material whose weaving is not deformed during the layup or very little.




Thanks,
Edited 10 Years Ago by Julien
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
You could try this:

Wet out a suitable piece of cloth on a release coated glass plate or a piece of polypropylene sheet.
use the slowest hardener with the resin, and make sure to get the CF wetted through.
Use a roller to squeeze out excessive resin and air bubbles.
Put the whole thing in a plastic bag and use your vacuum pump to get as much air out as you can without pulling enough vacuum to disturb the weave on the plate,

Make several and put them in the freezer until you need it ...  thaw it  before use, keeping an eye on it, until it has the desired "consistency"
it will be a lot less sticky/gooey than when wetting it and quite stiff, and will not distort unless you work it really hard.

Lay this first layer in your mould  (taking care to keep the weaves nice and straight... then lay up the rest of the layers, and vac bag....)

I'v only done this once, and it worked a treat, but it is NOT easy. The cold resin warms up quite fast, gets sticky and the weave starts to distort.

Good luck..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search