kerob_labs
kerob_labs
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 17
Hello all!
I have never done anything with molding, GRP, CF, nothing, so I think it's time to add that to my set of skills!!
For the start, I found quite interesting in woven glass fabric offered my easycomposites and advantages over chopped strand mat. I wonder if it's possible to give me some idea of layup for a car body please, some advise in how many layers of woven glass fabric should be recommended, or perhaps a combination of 100g + 300g? Would I need core material?
The project I would be looking at is a car bodywork with somewhere like 3.6mts length, 1.7mts width and 1.2mts height on top of a space frame chassis.
I'm not sure I provided enough information to have an answer, or my question is too vague, so please you can help me to improve my question (sounds weird isnt it?)
Many Thanks,
Marcio.
Tags
Woven Glass Fabric
Reply
Like
5
Replies
ChrisR
ChrisR
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
It all depends on the application, I know of a race car that using 2 layers of scrim, the paint nearly weighs as much as the bodywork, but you certainly don't want to lean on it or nudge someone whilst on track!
There are some good books on it (to get an idea of what's needed) try "Competition Car Composites"
Reply
Like
6
kerob_labs
kerob_labs
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 17
Thanks, I will search for some books! It's actually for a street car, nothing too fancy (nor fast).
I saw a number of YouTube videos showing chopped strand mat, but I'm curious about using woven glass fabric instead, so for a street car, how many layers, core material, resin, gelcoat? 100g + 300g layers? Maybe then a 25g on top to finish? Is it like laying chopped mat? This kind of thing...
Thanks,
Marcio.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Questions about Woven Glass Fabric
kerob_labs
-
11 Years Ago
It all depends on the application, I know of a race car that using 2 layers of scrim, the paint...
ChrisR
-
11 Years Ago
Thanks, I will search for some books! It's actually for a street car, nothing too fancy (nor fast)....
kerob_labs
-
11 Years Ago
The layup will vary again with the shape and type of panels. eg flat panels, curved panels, doors,...
Warren (Staff)
-
11 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search