The layup will vary again with the shape and type of panels. eg flat panels, curved panels, doors, boots etc.  There is no one guide that works for everything.  If its for road use you will want it thicker than for track/drag use.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
kerob_labs
kerob_labs
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 2, Visits: 17
Thanks, I will search for some books! It's actually for a street car, nothing too fancy (nor fast).

I saw a number of YouTube videos showing chopped strand mat, but I'm curious about using woven glass fabric instead, so for a street car, how many layers, core material, resin, gelcoat? 100g + 300g layers? Maybe then a 25g on top to finish? Is it like laying chopped mat? This kind of thing...

Thanks,

Marcio.
ChrisR
ChrisR
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
It all depends on the application, I know of a race car that using 2 layers of scrim, the paint nearly weighs as much as the bodywork, but you certainly don't want to lean on it or nudge someone whilst on track!

There are some good books on it (to get an idea of what's needed) try "Competition Car Composites"
kerob_labs
kerob_labs
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 2, Visits: 17
Hello all!

I have never done anything with molding, GRP, CF, nothing, so I think it's time to add that to my set of skills!!

For the start, I found quite interesting in woven glass fabric offered my easycomposites and advantages over chopped strand mat. I wonder if it's possible to give me some idea of layup for a car body please, some advise in how many layers of woven glass fabric should be recommended, or perhaps a combination of 100g + 300g? Would I need core material?

The project I would be looking at is a car bodywork with somewhere like 3.6mts length, 1.7mts width and 1.2mts height on top of a space frame chassis.

I'm not sure I provided enough information to have an answer, or my question is too vague, so please you can help me to improve my question (sounds weird isnt it?) 

Many Thanks,

Marcio.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search