Carbon fibre engine case covers


Author
Message
Tommy
Tommy
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 2
Hi,

I need to make some carbon fibre engine case covers to fit over my existing engine side cases on my motorcycle.  They need to be able to withstand high temperatures 100c to 110c.  
I have attached a picture of what one of the pieces i need to cover.  The cover i am planning to make would fit snugly over it as a protective skin.  
What would be the best way to go about it?  I have a spare engine case which i could make the carbon fibre piece on, but i dont want it to stick to that cover.  
Which kit would be better to use?

Any help would be much appreciated,
Tommy.
Attachments
image.jpg (279 views, 63.00 KB)
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Make your mold,use sheet 1 mill thickness,use unimold post cure 100c. Then use pre preg.thats what I would do.
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
I mean sheet wax to give you Clearence over engine cover.
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Tommy
A thin layer of carbon will give very little impact/abrasion resistance when used for your engine cover, if its for more than just aesthetic purposes it should be quite thick and preferably have some Kevlar in the stack.
Regards Chris
Carbon fibre works LTD   

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png