i will do my first infusion on more complex mold. mirror cap
it is a split mold.

so question is: should i use envelope bag or not.
if not, how can i seal the split?

http://www.talkcomposites.com/Uploads/Images/ae7219ca-8b3b-48e2-9584-a9f5.jpg
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Envelope bag is a no brainer for such a small part.

You can seal the edges using gum tape, any bleed through only going as far as the gum tape.  Some people prefer to smear silcione sealant before joining the halves together.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh I prefer silicon myself, I hate bagging tape. 

I usually try to do my split moulds in the regular fashion with silicon sealing the join, and if I can't get a seal I envelope bag the whole lot. 
tomzi1234
tomzi1234
Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)
Group: Forum Members
Posts: 40, Visits: 500
thanks for advice.

i will try to seal the split with silicon.