Group: Forum Members
Posts: 79,
Visits: 1.3K
|
Following on from Warrens comments.
When i started out I had a part screw up due to my mixing ( I think) ratio not being accurate enough. I then proved to my self many times that the digital scales I was using weren't accurate when slowly, gently dripping liquid onto them. I could add more than a full teaspoon full worth of liquid and the scales did not register. They were meant to be accurate to 0.1 gram.
So I bought another set of different digital scales and they did the same....
Then I bit the bullet and spent about £120 on scales that were accurate to 0.01 grams (max limit is 1.2kg i think). Temperature compensated as well. These are great for mixing small batches of resin. Never had any problems since then.
Craig
|