I have been working for a customer/friend on a new shell for his hill climb/sprint car. The plug is based on a Reliant Kitten shell. The new additions have been built up from ply and Kingspan boards followed by a layer of 450 CSM. A week of applying and sanding filler has resulted in a nice flat surface ready for 2K high build primer followed by 2k direct gloss. Then I shall start adding flanges, it will require an eight piece mould plus wheel arch returns. The final shell will be done in full carbon.

Warren

















Carbon Copies Ltd
Attachments
Kitten 1.JPG (1.3K views, 987.00 KB)
Replies
Brian2fast
Brian2fast
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
That looks brilliant. Smile

How many layers of glass have you used?

How did you manage to layup the overhanging wheel arches?

You have a very luxurious workshop, fancy carpet and everything. I've got a 1 mtr square bit that I have to move about with me, haha.

Craig
Edited 12 Years Ago by Brian2fast
wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Brian2fast (22/12/2014)
That looks brilliant. Smile

How many layers of glass have you used?

How did you manage to layup the overhanging wheel arches?

You have a very luxurious workshop, fancy carpet and everything. I've got a 1 mtr square bit that I have to move about with me, haha.

Craig


Sorry Craig missed your post. As this is really a one-off mould we only used 2 layers of 450 on the main areas with some localised bracing and 3 layers on the flanges. As it turns out I don't thing we would have got the thing off the plug if it had been any thicker. 
The posh workshop is Andrew the customers garage so can't take credit for that.Smile

Carbon Copies Ltd
Edited 12 Years Ago by wozza
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
wozza - 12 Years Ago
wozza - 12 Years Ago
Brian_s - 12 Years Ago
Warren (Staff) - 12 Years Ago
wozza - 12 Years Ago
davro - 12 Years Ago
FLD - 12 Years Ago
ChrisR - 12 Years Ago
wozza - 12 Years Ago
Brian2fast - 12 Years Ago
wozza - 12 Years Ago
scottracing - 12 Years Ago
wozza - 12 Years Ago
Hanaldo - 12 Years Ago
wozza - 12 Years Ago
Brian2fast - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
unijacko67 - 12 Years Ago
wozza - 12 Years Ago
unijacko67 - 12 Years Ago
Brian2fast - 11 Years Ago
unijacko67 - 11 Years Ago
Brian2fast - 11 Years Ago
unijacko67 - 11 Years Ago
unijacko67 - 11 Years Ago
scottracing - 11 Years Ago
unijacko67 - 11 Years Ago
unijacko67 - 11 Years Ago
Warren (Staff) - 11 Years Ago
unijacko67 - 11 Years Ago
unijacko67 - 11 Years Ago
carbonfibreworks - 11 Years Ago
unijacko67 - 11 Years Ago
Jacopo Carbonio - 11 Years Ago
wozza - 11 Years Ago
unijacko67 - 11 Years Ago
unijacko67 - 11 Years Ago
tomzi1234 - 11 Years Ago
unijacko67 - 11 Years Ago
scottracing - 11 Years Ago
unijacko67 - 11 Years Ago
davro - 11 Years Ago
unijacko67 - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search