I have been working for a customer/friend on a new shell for his hill climb/sprint car. The plug is based on a Reliant Kitten shell. The new additions have been built up from ply and Kingspan boards followed by a layer of 450 CSM. A week of applying and sanding filler has resulted in a nice flat surface ready for 2K high build primer followed by 2k direct gloss. Then I shall start adding flanges, it will require an eight piece mould plus wheel arch returns. The final shell will be done in full carbon.

Warren

















Carbon Copies Ltd
Attachments
Kitten 1.JPG (1.2K views, 987.00 KB)
Replies
Brian2fast
Brian2fast
Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)Supreme Being (631 reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
Brilliant!

I like the wheel arch extensions.

Will the final carbon shell be one single part? You doing the doors as well?
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Brian2fast (04/11/2014)
Brilliant!

I like the wheel arch extensions.

Will the final carbon shell be one single part? You doing the doors as well?


The final shell will be in one piece. We did think about doing it in front and rear clams but because lightness is the aim we opted for a one piece to help with strength.
The bottom halves of the original doors are now part of the new shell, again to add strength. New door patterns and moulds will be made to fit once the shell is done.
Just the beginning of a long journeySmile

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
wozza - 11 Years Ago
wozza - 11 Years Ago
Brian_s - 11 Years Ago
Warren (Staff) - 11 Years Ago
wozza - 11 Years Ago
davro - 11 Years Ago
FLD - 11 Years Ago
ChrisR - 11 Years Ago
wozza - 11 Years Ago
Brian2fast - 11 Years Ago
wozza - 11 Years Ago
scottracing - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Brian2fast - 11 Years Ago
wozza - 11 Years Ago
wozza - 11 Years Ago
wozza - 11 Years Ago
unijacko67 - 11 Years Ago
wozza - 11 Years Ago
unijacko67 - 11 Years Ago
Brian2fast - 10 Years Ago
unijacko67 - 10 Years Ago
Brian2fast - 10 Years Ago
unijacko67 - 10 Years Ago
unijacko67 - 10 Years Ago
scottracing - 10 Years Ago
unijacko67 - 10 Years Ago
unijacko67 - 10 Years Ago
Warren (Staff) - 10 Years Ago
unijacko67 - 10 Years Ago
unijacko67 - 10 Years Ago
carbonfibreworks - 10 Years Ago
unijacko67 - 10 Years Ago
Jacopo Carbonio - 10 Years Ago
wozza - 10 Years Ago
unijacko67 - 10 Years Ago
unijacko67 - 10 Years Ago
tomzi1234 - 10 Years Ago
unijacko67 - 10 Years Ago
scottracing - 10 Years Ago
unijacko67 - 10 Years Ago
davro - 10 Years Ago
unijacko67 - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search