Replacement boat deck.


Author
Message
Stepto
Stepto
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Awaiting Activation
Posts: 7, Visits: 54
Hi there. After some advice regarding a project I'm starting. I run a small offshore race boat of a catamaran design. Between the two hulls is a flat deck of around 1m wide by 2m in length. It was made of 10mm marine ply wrapped in a glass fibre mat and finished with gelcoat. It comprises of three panels.  This broke last year due to the impacts of the two passengers landing on it and the ravages of time. The deck does take a beating as it also has the fuel tank strapped to it. I'd like to replace the deck with some boards that have the same or better strength as the plywood but be as light as possible. I'm looking at using 10mm foam board with outer layers of glass fibre matting and a resin topcoat. Will this be suitable and as strong? Thanks very much. Any advice would be greatly appreciated. Steve. 
Reply
Stepto
Stepto
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Awaiting Activation
Posts: 7, Visits: 54
Thanks for the advice. And I know just what you mean, I keep coming back to that conclusion myself. 
My only thought is to use a lightweight ply instead of marine ply as this may save a few pounds. 
I'd love a really lightweight deck though as it makes such a difference to acceleration and top speed. Not giving up just yet. May have to do some strength/impact tests. 
Thanks again. 
Edited 11 Years Ago by Stepto