I would say... if you do not want to spend too much on this, then plywood, glass and polyester ...
If you are willing to spend a bit on it, and want it lightweight, then I would go for foam core + 2 x 4 layers of woven glass + Carbon/kevlar or Twaron/CF.
maybe build it up asymmetrically, with 3 layers 200gsm on the bottom side and 5 on the top (deck) .. It should be more than strong enough, especially with a few layers of Kevlar/CF in there.
That will not be cheap, however ... you would need 16 sq. meters of CF/Kevlar + E-glass + 2 sq. meters of foam core ... add resin and consumables to that (Peel-ply, etc. ) and you will hit + £200