Ray Rogers
Ray Rogers
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 18,
Visits: 79
I wish to replicate some vehicle amber indicator lenses. I assume I will make the mould from silicone rubber. What is the best casting material for these please?
Reply
Like
10
brainfart
brainfart
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 198,
Visits: 1.4K
www.alumilite.com/PDFs/Printables/How%20to%20make%20molds/Tail-Light-Molding-with-Equipment.pdf
www.alumilite.com/PDFs/Printables/How%20to%20make%20molds/Tail-Light-Molding-with-out-Equipment.pdf
http://www.smooth-on.com/gallery.php?galleryid=232
Reply
Like
10
Ray Rogers
Ray Rogers
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 18,
Visits: 79
Many thanks. What will be the best casting material from the Easy Composites range please?
Reply
Like
9
brainfart
brainfart
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 198,
Visits: 1.4K
None. They don't carry any polyurethane casting resins.
Reply
Like
9
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
There are two listed on the EC site and a range of translucent pigments. Give technical a ring to see which one fits your requirements best.
Carbon
Copies Ltd
Reply
Like
10
Matt (Staff)
Matt (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
[THANKS WARREN]
Hi Ray,
I believe you're now in contact with my colleague Rich in our technical department and that you're aware we have a
Water Clear Polyurethane Casting Resin
which would indeed be ideal for you and also that you're going to have a go with our
Water Clear Polyester Casting Resin
as a more cost effective trial whilst you familiarise yourself with the process.
In both instances, done right you could get some great results casting these parts in water clear resin but, as you'll find out, water clear casting is more 'fussy' than most casting processes and will expose issues to do with air entrapment, cure temperature and moisture presence more than most.
Rich has suggested our
Addition Cure Silicone Rubber
for the mould itself. Condensation cure rubbers (like our
CS2
) don't work well at all for water clear casting because they harbour moisture which will react with the clear resin resulting in a tacky surface to the mouldings and can exaserbate air entrapment. Whilst the water clear polyester can be cast without the need to degas; when you make the transition to the polyurethane you will need to
degas the resin
to get a bubble-free perfect casting.
I hope this helps and look forward to working with you.
Matt
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Tags
polyester
polyurethane
silicone
water clear
Edited
12 Years Ago by
Matt (Staff)
Reply
Like
8
brainfart
brainfart
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 198,
Visits: 1.4K
Ooops. Never saw that resin, I assume it's relatively new inventory?
Reply
Like
9
Matt (Staff)
Matt (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
The polyester is a newer addition (added at the start of this year) however the waterclear PU was in fact one of our launch products over 3 years ago. In fairness though, casting resins live in their own part of the website and so if you're dealing mainly with laminating and infusion resins (or tooling resins/gels) then you wouldn't necessarily come across the casting resins.
--Matt
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search