I wish to replicate some vehicle amber indicator lenses. I assume I will make the mould from silicone rubber. What is the best casting material for these please?
brainfart
brainfart
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
www.alumilite.com/PDFs/Printables/How%20to%20make%20molds/Tail-Light-Molding-with-Equipment.pdf
www.alumilite.com/PDFs/Printables/How%20to%20make%20molds/Tail-Light-Molding-with-out-Equipment.pdf

http://www.smooth-on.com/gallery.php?galleryid=232
Ray Rogers
Ray Rogers
Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)Supreme Being (232 reputation)
Group: Forum Members
Posts: 18, Visits: 79
Many thanks. What will be the best casting material from the Easy Composites range please? 
brainfart
brainfart
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
None. They don't carry any polyurethane casting resins.
wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
There are two listed on the EC site and a range of translucent pigments. Give technical a ring to see which one fits your requirements best.

Carbon Copies Ltd
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
[THANKS WARREN]

Hi Ray,

I believe you're now in contact with my colleague Rich in our technical department and that you're aware we have a Water Clear Polyurethane Casting Resin which would indeed be ideal for you and also that you're going to have a go with our Water Clear Polyester Casting Resin as a more cost effective trial whilst you familiarise yourself with the process.

In both instances, done right you could get some great results casting these parts in water clear resin but, as you'll find out, water clear casting is more 'fussy' than most casting processes and will expose issues to do with air entrapment, cure temperature and moisture presence more than most.

Rich has suggested our Addition Cure Silicone Rubber for the mould itself. Condensation cure rubbers (like our CS2) don't work well at all for water clear casting because they harbour moisture which will react with the clear resin resulting in a tacky surface to the mouldings and can exaserbate air entrapment. Whilst the water clear polyester can be cast without the need to degas; when you make the transition to the polyurethane you will need to degas the resin to get a bubble-free perfect casting.

I hope this helps and look forward to working with you.

Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 12 Years Ago by Matt (Staff)
brainfart
brainfart
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
Ooops. Never saw that resin, I assume it's relatively new inventory?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
The polyester is a newer addition (added at the start of this year) however the waterclear PU was in fact one of our launch products over 3 years ago. In fairness though, casting resins live in their own part of the website and so if you're dealing mainly with laminating and infusion resins (or tooling resins/gels) then you wouldn't necessarily come across the casting resins.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search