Unfortunately none of the two pumps are very good for Vac-bagging or Infusion ... They simply can not produce low enough vacuum, even if the big one can move a lot of air.
To get low enough vacuum, you need to buy an Oil-based vacuum pump, like the ones from EC..
I have a very small laboratory pump, that takes ages to empty out the bags, but it does very low vacuum -0.995 Bar ..
It struggles a bit to keep up when infusing larger parts, but it works fine.