Hi

I am an absolute rank amateur with no previous experience other than a few GF/GRP Moulds at school (a long time ago).

In Order to keep my question simple I wont go into the detail of what I am trying to do but the closest thing I can suggest is if I wanted to build a CF caravan (yes the thing you tow) and I get that I can buy some flat sheets of sandwich and stick them together and end up with a very square caravan but I am thinking a bit more adventurously than that.

So here goes... I would like to build a caravan and I assume (but ask the question anyway) is it practical to build a BIG box using vacuum induction forming techniques or do I have to create it in sections and I have a fairly good understanding of bonding and area vs. strength and concepts like tensile strength and stressed members, but what I don't get is where I start. For example do I plan to build a nose-cone and tail then fill the middle in with square flat sheets?

If I go down that route how do i get the right strength / cost ratio and on a practical note - how do I fit doors and windows? 

I also assume I'd need a big thick sandwich construction floor and am thinking about honeycomb but I don't seem to be able to find anything that tells me how to construct a section of rigid panel using the honeycomb.

Any thoughts?

PS I appreciate this size/scale isn't something a beginner should be having a go at, but it's the only thing I'm interested in building at the moment! 

PPS - just watched the video of the indian guys building a 42ft boat in one go so it must be do-able if very complicated!
Replies
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi.

Ok, I dont know anything about caravans, but doesn't it need some structure to maintain it?

I mean, a structure (not only the chassis itself) on which panels are set (screws, glue, rivets, whatever) ?

Then if its the case, I would build an aluminium structure on which I set my panels.

But okay it depends the size, shape etc. Maybe a few pics of what you want would help us giving the best advices we can.

Must be waaayy cool to stare at carbon fiber when in the bed... no wonder you would have sweet dreams Wink

 



 


    A $1000 electronic device will always protect a 10 cents fuse
downforce
downforce
Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)
Group: Awaiting Activation
Posts: 6, Visits: 23
Well I have seen a carbon-fibre monocoque (?) vehicle frame that didn't have any (metal) frame.

So I guess it depends on the thickness/layup of the body.

As I mentioned I did also consider using honeycomb core for stiffness - I guess that would be strong enough to not need a frame ?

DF
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search