Group: Forum Members
Posts: 156,
Visits: 14K
|
Very nice work,rich iam in the process off sorting a effecient oven out,but got impatience and post cured an old mold to test.and put in an old oven with no vaccum connecting into oven,just bagged the part came out pretty good a few pin holes not many.iam used to infusion,so pre preg is a lot nicer to work with,regarding curing,the material your using,could you advise on tempreture curing procedure any advise welcome.
|