Tank looks very nice.

are you putting petrol straight into the finished carbon or do you need a coating on the inside.

also do you feel safe using a pure carbon tank to hold the fuel with regard to crash damage.
JRT
JRT
Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)
Group: Forum Members
Posts: 13, Visits: 130
Awesome work!
morepower
morepower
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Before bonding the two parts are dry fitted to make sure it has an overlap but does not spread the tank open more than the original 

http://www.talkcomposites.com/Uploads/Images/9d758c27-812f-4c21-838d-2afe.jpg

The tank is now bonded and you can see the finished weight.. The original one was 4.5KG
http://www.talkcomposites.com/Uploads/Images/4c8a2b15-8e42-491d-8139-545a.jpg
JRT
JRT
Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)
Group: Forum Members
Posts: 13, Visits: 130
Wow. that looks awesome! Can you post a picture of the tank after it's all done and sealed down? The pic you've posted is just the top and the sides of the outshell or is it the complete one?

I'm looking forward to do a Africa Twin tank but I'm still too new to CF and all the process to try it out.
Edited 12 Years Ago by JRT
morepower
morepower
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Cure cycles are hard to pin down.. It depends on the oven, mould, material and may need some testing. I would suggest getting a ramp and dwell controller ( a rework controller for electronics rework stations work but need a little thinking about as they usually only work in seconds per sector so you may be limited to 8 sectors at 9999 seconds each.) I am using one myself and have a 3 stage cycle with a lower temp first and a ramp speed of about 1 degree per minute then a dwell set before going up to the next step again at 1 degree per minute, dwell and then the final temp at 1 degree per minute to complete the final cure stage. 

I spent about 6 months testing materials and cure cycles to perfect mine. The dwell lets the mould catch up with the oven and I keep it below the lowest suggested cure temp for a while before the final stage goes into the actual cure temp and cure duration. 
Shaneer22
Shaneer22
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Very nice work,rich iam in the process off sorting a effecient oven out,but got impatience and post cured an old mold to test.and put in an old oven with no vaccum connecting into oven,just bagged the part came out pretty good a few pin holes not many.iam used to infusion,so pre preg is a lot nicer to work with,regarding curing,the material your using,could you advise on tempreture curing procedure any advise welcome.
morepower
morepower
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Shaneer22 (18/11/2014)
Can I ask what pre pre you are using.


It is still under a development number at SHD at the moment. If you contact them and ask for Glenn he will let you know if you let him know Rich from P3 told you to call him... 

Anyway here are a few more photos... I made the mould more of a satin on purpose is it looks a little dull and there is still some release residue on there too..



Shaneer22
Shaneer22
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Can I ask what pre pre you are using.
morepower
morepower
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Hanaldo (18/11/2014)
Going to look very nice I'm sure. Your method of doing the filler cap is what impresses me the most. I must learn to do this, I really hate secondary bonding. 


Thank you...
I do the same for the fuel cap and the front tank mount.. It is easy and really cheap if you use T Nuts instead of Big Head fasteners, I can buy a box full of assorted sizes for the cost of 2 or 3 big heads. 
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Going to look very nice I'm sure. Your method of doing the filler cap is what impresses me the most. I must learn to do this, I really hate secondary bonding. 