Not normal vac bag as such, seems very stretchy possibly a clear silicone as they aren't using any release
wouldn't suprise me if its something they have found via trial and error and its not really a composite product as such
Brought back a few memories ,I did a couple of pairs of boots about 20yrs ago for a speed skater. They were mainly Kevlar with a little carbon but that was all hand lay but I only did the bases leaving the Kevlar 5"long an un laminated and they then went off too a guy who did the leather uppers and would sew the uppers to the dry kevlar
|