My shop's Demo Car CFC Corvette & Bike BMW S1000RR


Author
Message
NikCFC
NikCFC
Supreme Being (837 reputation)Supreme Being (837 reputation)Supreme Being (837 reputation)Supreme Being (837 reputation)Supreme Being (837 reputation)Supreme Being (837 reputation)Supreme Being (837 reputation)Supreme Being (837 reputation)Supreme Being (837 reputation)
Group: Forum Members
Posts: 61, Visits: 871
Hey guys, after 4+months and 800+ Labour hours of really hard work I present you my Demo Creations the 1st in the world Full Carbon Corvette C5 and our Racing BMW S1000RR.

Both made via Vac.Infusion, post cured in an oven and coated with High Quality Automotive Clear Coat!

Check the V pattern on both Wink

http://www.carbonfibercustoms.com/photos/Auto/Corvette/CFC%20Carbon%20Corvette%207.jpg

http://www.carbonfibercustoms.com/photos/Auto/Corvette/CFC%20Carbon%20Corvette%206.jpg




http://www.carbonfibercustoms.com/photos/Auto/Corvette/CFC%20Carbon%20Corvette%203.jpg

http://www.carbonfibercustoms.com/photos/Auto/Corvette/CFC%20Carbon%20Corvette%204.jpg

http://www.carbonfibercustoms.com/photos/Auto/Corvette/CFC%20Carbon%20Corvette%201.jpg

http://www.carbonfibercustoms.com/photos/Auto/Corvette/CFC%20Carbon%20Corvette%202.jpg






















Edited 12 Years Ago by NikCFC
FLD
FLD
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Thats pretty awesome stuff!  Must've cost a small fortune to do both of them.  Can I ask if you've measured the weight differences?
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Looks amazing!

The detailing on the bike with the spread tow carbon is awesome.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
prsw
prsw
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Skilled as hell, great job.


http://motoform.blogspot.se

davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Amazing work! attention to detail is stunning, very inspiring

Would love to see some of the moulds.



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search