By NikCFC - 10/31/2014 1:41:29 AM
Hey guys, after 4+months and 800+ Labour hours of really hard work I present you my Demo Creations the 1st in the world Full Carbon Corvette C5 and our Racing BMW S1000RR.
Both made via Vac.Infusion, post cured in an oven and coated with High Quality Automotive Clear Coat!
Check the V pattern on both 









|
By davro - 11/11/2014 8:11:17 PM
Amazing work! attention to detail is stunning, very inspiring
Would love to see some of the moulds.
|
|