Use different gelcoat for other half of mould?


Author
Message
Timellis
Timellis
Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)
Group: Forum Members
Posts: 14, Visits: 58
I am having finish issues on my pattern and mould when using Unimold gelcoat. The first time the part was finished in clear lacquer form Halfords. The part was easy leased and then waxed 8 times. When de-moulded the finish on the part had alligatored leaving a poor quality mould. The second time had 2k lacquer finish, again easy lease and wax with the same result.

My question is can I use your epoxy tooling gelcoat for this half of my mould? (the first half has been repaired extensively from alligatoring) - I am looking at the "green stuff" you have. Also, what finish do you suggest for my part?

Thanks in advance.
Edited 11 Years Ago by Timellis
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search