I have finally finished my 2m x 2m x 2m oven with internal vac lines etc and plan to start to use Easy-Preg Surface Layer and Vari-Preg pre-preg carbon fiber material.

I understand that the Easy-Preg needs to be cured at 100'c > however the Unimold system is rated up to 90'c

What would be the ideal mould to use for this?
Reply
richardstock
richardstock
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Awaiting Activation
Posts: 3, Visits: 28
Warren (Staff) (31/10/2014)
We have had a couple of customers say they have got higher temperatures with Uni-Mould than the data suggests.  We are going to do some additional tests, in the next few weeks, with an old mould and some pre-preg to see how high we can go with the system.


That would be fantastic Smile