Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pre-Pregs
»
Pin hole free material.... I have been given a new material to test......
Pin hole free material.... I have been given a new material to test...
Post Reply
Like
5
Prev
1
2
3
4
5
Next
Jump To Page
Pin hole free material.... I have been given a new material to test...
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
20_rc51_00
20_rc51_00
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
Any news down the pipeline?
Reply
Like
4
morepower
morepower
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
I will send you a PM....... You may be able to get some now... The composites show is soon and I think it is perfect now so they may supply some but I cannot promise anything...
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
send me a pm too if possible
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
4
tack talk
tack talk
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 215
I would appreciate a PM also if possible
Reply
Like
3
morepower
morepower
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
I am seeing if they have some to send out...... They do not have test samples so it may mean a 10m minimum but if there are a few who want to try it I may be able to talk them into sorting out a few meters which they can use...
Reply
Like
4
morepower
morepower
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
I spoke to the manufacturer and it looks like they will make up a roll for some sample/short rolls to be cut from it for you guys..... They cannot do it as free samples but it would be done for a good price.... 2 or 3 meters on a roll for you to test... It is amazing stuff.
Reply
Like
4
morepower
morepower
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
Just pulled these out of the mould today.... Not bad.... No pinholes..
Reply
Like
3
20_rc51_00
20_rc51_00
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
those look nice!
Reply
Like
4
gp composites
gp composites
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 1,
Visits: 24
Also please PM me about possibility to order some samples. No matter if its free or 10m
Reply
Like
3
Shaneer22
Shaneer22
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 156,
Visits: 14K
Why the secret with the supplier.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Prev
1
2
3
4
5
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search