EC's "Water clear Polyester casting resin" will probably be the cheapest way, and very strong, but being a polyester it will smell for some time.
EC's Water clear Polyurethane casting resin may also fit the bill, but it is much more expensive.
The best I've ever used was "Wessex Resins Permakote" which is a water clear Epoxy ... but how much better it is than the EC Polyurethane, i have no idea. price seems to be about the same..