So I am planning on making a R32 GTR N1 Boot Lip links to pictures are below. I am wondering how other people would go about making this as it needs to have a flat bottom to attach to the car using either a double sided tape or some form of glue. I don't have a vacuum pump either and as this will be made from carbon fibre I was wondering how I go about keeping the shape. I was thinking possibly making a mould for the piece then create a foam inset that would sit in the mould which the carbon would wrap around that way I would be able to keep the piece really light if anyone has any ideas please let me know.



http://www.topstage.com/wp-content/uploads/2011/10/S13-N1-Boot-lip1.jpg

http://justjap.com/media/catalog/product/cache/1/image/8f3e5969ec19f7e2d1880fae742b658d/n/1/n1carblip32_1.jpg
aza993a
aza993a
Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)Supreme Being (156 reputation)
Group: Forum Members
Posts: 10, Visits: 91
Fillet, pull mold. 2 part mold if you want a flat bottom, just use the existing flange or even the boot lid for the shape.
Edited 12 Years Ago by aza993a
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search