Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Resins, Gelcoats and Pigments
»
Cloudy gelcoat
Cloudy gelcoat
Post Reply
Like
2
Cloudy gelcoat
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
CATFabs
CATFabs
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 19
On a couple of projects i have noticed a cloudiness in the gelcoat..what causes this and how can i avoid it?
Reply
Like
2
Paul (Staff)
Paul (Staff)
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 134,
Visits: 614
Cloudiness can be caused by a couple of factors;
Unclean Tools
- Perhaps a obvious one but if the brushes or rollers are not completely clean (and dried of acetone) this can easily contaminate the gel.
High Humidity
- Working in very high humidity can cause this problem the resin is hydroscopic and can absorb water out of the air, as can the resin if left to the open air before it's mixed, always ensure that the lids are securely in place, this is especially important for the hardener.
Inaccurate resin-hardener ratio
- This would have to be a way off to cause cloudiness, but make sure that it is weighed out as accurately as you can.
Coat too thick
- This is probably the most likely of the causes, the gel should be applied as thinly and evenly as possible, all gels have a degree of cloudiness naturally but if applied in a very thin coat this should not be noticable. If the coat is too uneven this finish will appear 'streaky' with the brush or roller strokes so try to be as even as you can be.
Paul Statham
Easy Composites / Carbon Mods - Technical
Reply
Like
2
CATFabs
CATFabs
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 19
Thanks.
I reckon im applying too thick a coat..the cloudiness is more apparent where it has sagged a bit into the recesses of the mould making it thicker.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics