By CATFabs - 4/15/2012 4:06:28 PM
On a couple of projects i have noticed a cloudiness in the gelcoat..what causes this and how can i avoid it?
|
By CATFabs - 4/19/2012 6:09:15 PM
Thanks.
I reckon im applying too thick a coat..the cloudiness is more apparent where it has sagged a bit into the recesses of the mould making it thicker.
|
|