interlocking carbon rod? wing joiners


Author
Message
dogzilla
dogzilla
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 2, Visits: 7
I need a 1meter length of carbon rod of 14-16mm od, with a paired tube slightly smaller which can slide inside the id of the larger rod to form a snug fit as part of a wing joiner for a model plane.

If I buy say a 14mm woven finish tube, with ID of 12mm, will I be able to slide a 12mm OD pulltruded rod inside without much difficulty? How uniform and accurate are the inside of these rods?