I have done what you are looking to do, but with the smaller sizes of pulltruded CF tubes from EC.
I found that I had to very lightly sand one of the sizes of "inner-tube" to get it to slide freely inside the outer tube, the other size matched perfectly.
I used 6, 8 and 10 mm pulltruded tubes.
I have not tried the woven finish tubes, but I did get a 25 mm woven-finish tube, and it is very accurately 23 mm inside diameter, so I guess you will be able to use a combination of the two
For my project, I laminated a CF fabric braided sleeve ( EC have these woven sleeves in several sizes )around the outer pulltruded tube to reinforce it radially, as the pulltruded tubes have very little strength radially.
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|