Hi Guys
This is what I am trying to source without any success.
I need a program to run on my laptop that allows me to set many heat -ramp-and soak settings for my prepreg that I use in my AutoClave.
The laptop must output to a controller and thermocouple.
I have looked at the many digital units but do not like the display of any of them. It is like watching a movie through a key hole.
I want to monitor and see the progress all the way through the cycles on the laptop display.
Thanks
Fred
 
Replies
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
Here's one of the more affordable options, it's available from several suppliers, so probably just another rebranded Chinese piece of junk, but at least it comes with 3 years warranty Wink

http://www.omega.co.uk/pptst/CN2300.html
http://www.omega.com/pptst/CN2300.html

Price adds up quickly if you buy all the goodies like logging, USB port for data download, ethernet, configuration software, remote setpoint...
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I'm sure there are some very high tech solutions like above.
But for me, as a true DIY guy Hehe , I was thinking about something like on following link.
http://idevicesinc.com/igrill/ Once I have some budget for some extras, Ill try it out

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search