Basil
Basil
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 13
I am currently using Schufler L285 resin with L286 hardener. According to the data sheets your EL2 resin has very similar properties in spite of being much cheaper.
Am I missing something or could I change to EL2 without any problems?
Reply
Like
3
Reply
Dravis
Dravis
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
I have to agree with "brainfart" to some extent...
Changing to a cheaper resin with similar properties is fine, if you are not depending on the approvals of the resins for aircraft or the like. On the issue of bulk buying, you may not save a lot of money buing a cheaper resin for the parts that needs no approval.
Its all in the balance of costs and amounts used..
Most of my composites work is experimental, I only produce very few "copies" of the parts I make, and most are "one off specials" made for myself and friends.
So in my case, I buy almost nothing in bulk, certainly not resins and hardeners, unless I really need it for larger projects. Especially hardeners, which certainly have a limited shelflife
So far I have tried several resin systems, and really found very little difference between them. This goes for structural strenght too, some of my parts have been built and used for structural tests, and in some cases we could not measure significant differences between identical parts made with different resin systems, case in point being a beam type part made for testing molded in Titanium fasteners.
it was made with both West systems 105, and EC EL2, giving nearly identical measurements, with maybe a slightly stronger result for the EL2
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Scheufler L285/6
Basil
-
11 Years Ago
It looks to me as if the EC EL2 resin is just as good and has just as good physical properties as...
Dravis
-
11 Years Ago
There are many cheaper systems which come close to the L285. > Am I missing something or could...
brainfart
-
11 Years Ago
I have to agree with "brainfart" to some extent... Changing to a cheaper resin with similar...
Dravis
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search