Papua New Guinea – Traditional Outrigger Canoe meets the 21st Century


Papua New Guinea – Traditional Outrigger Canoe meets the 21st Century
Author
Message
Jacobsen
Jacobsen
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 3, Visits: 932

Good evening all,

I am a young guy from Denmark who has a background from the wind turbine industry where I have worked with the development of new wind turbine blades, the biggest being 75 meters long and weighing more than 20 tons.

Recently I mocved to Papua New Guinea to work for a Balsa company who supplies balsa to several of the wind turbine manufactures.

Every afternoon I see the local fishermen going out to fish in their traditional outrigger canoes. Each tribe has there own distinct design but all seem to be very seaworthy as we often see them far out to sea when we go trolling for Marlin.

Normally the canoes are made from big logs from the rainforest. But this makes them heavy and over time they will deteriorate. Therefore, I will try and make a couple of canoes out of whole balsa logs and glass fiber. So basically, I will get a carver to make a canoe out of one 3 meter long piece of balsa and then wrap it in glass fiber afterwards.  

I have already found a carver (Peter) and the first two logs have been drying for three weeks in the kiln.

I anticipate the following problems with the project: 

  • Drying the balsa logs withoutcreating to many cracks. Normally when you dry the whole log it will crackalong the pith in the center of balsa log. This will make it difficult for thecarver to make a complete canoe out of one piece of wood.
  • Wrapping the completed canoe inglass fiber without creating wrinkles when vacuum is applied. I still have notfigured out exactly how I am going to pack the glass fiber around the balsacore. Especially the inside will be difficult. I may need to find some kind ofspray glue that can hold it in place while I pack the glass fiber. 
  • Resin infuse the cano withoutgetting dry spots and without drilling hundreds of holes through the balsacore.
  • Getting resin to Papua is challengeas it is considered dangerous goods, and all internet shops seem to use airfreight.  

So I willbe using this forum to try and find some solutions to these challenges and maybe help others with theirs if I can Smile

 

 


Edited 11 Years Ago by Jacobsen
Reply
Blackrat
Blackrat
Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)
Group: Forum Members
Posts: 20, Visits: 85
im sorry to hear that Sad

so the only thing the glass will be doing is making the balsa water proof ?