So a single layer of Easy Preg surface layer with no backing? If so you may find that is causing your problem. I've tried knocking up single layer parts and it seems there isn't quite enough resin so you get either pinholes or it looks like the resin surface layer seperates from the carbon slightly. Add the backing layer and there seems to be enough resin to stop this happening.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|