Hi Warren I'm the chap that went outside to look at your bonnet on your car in the car park if you can remember. ..... anyways as you can see the predicament I'm in with my recent post"...The pre preg I'm useing is the easypreg surface layer..." please mate with your wealth of knowledge could you advise
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
So a single layer of Easy Preg surface layer with no backing?  If so you may find that is causing your problem.  I've tried knocking up single layer parts and it seems there isn't quite enough resin so you get either pinholes or it looks like the resin surface layer seperates from the carbon slightly.  Add the backing layer and there seems to be enough resin to stop this happening.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ice2T
ice2T
Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)
Group: Forum Members
Posts: 7, Visits: 159
Ok my friend , ill give it a shot makes sense.....cheers