Group: Awaiting Activation
Posts: 1,
Visits: 2
|
Good morning I need to mould some connection pieces for attaching a rotary brush to a water fed pole. I will use the carbon fibre sleeves to reinforce, but have no experience of the type of resin needed to achieve the best strength. I have done a test with Fast Cast and a thin polyester mat, and it seems successful. Fast Cast is quite liquid, and I find that useful. Would an epoxy still have the same, or approximately the same viscosity? The connectors have coarse threads. Thank you in advance Francois Moal
|