ajb100 (11/08/2014)
Did you run the vac bag through the middle of the mould so the bag was pushing against the carbon? It looks like you've just envelope bagged it? That would explain the poor surface Finish. When using pre preg, you should be able to get the same results as infusion for surface finish




Did you read my posts or just look at the pictures?
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
I have read your post and looked at the pictures. It does not say or show if you bagged through the cavity of your piece or not.
 If you want help and advice you will find it helps to be curtious.
If you did not bag through the cavity there is nothing to compress your pre-preg, holding it in place and making the resin flow.

Brian.
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
I did bag it and pulled the bag through the cavity. It's irrelevant though because the bag burned through in the oven and lost vacuum twice. I typed this out on the previous page. I lost vacuum twice because the bag burned through...the second time I even insulated it in wax paper and the bag still burned through.
Edited 11 Years Ago by BlackNDecker
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
I read that it had burned through. But you had not mentioned that the bag went through the inside as it should. You may have just bagged the outside.

Brian.
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
It's not surprising the bag burned through, your oven isn't really big enough for that size part and you shouldn't really rest it on a metal tray either as this may create a hot spot where it touches.

Is the oven you are using just a plain domestic oven or have you modified it so you can control the cure temp better? - prepregs require quite precise ramp rates and dwell periods to allow the resin to flow properly.
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Did you post cure your mould before you put the release on for the pre preg ?

You need to burn the styrene out,if not when you cure the styrene comes out on your first cure taking your release with it

Normal household oven is ok to cure for a cure on a item like this but if you were to do another you really need a separate internal bag joined onto your outer bag rather than trying to push your outer bag down into the mould
asmasm
asmasm
Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)
Group: Forum Members
Posts: 15, Visits: 189
Shouldn't you be copying the internal surface of the original manifold and not the external surface?
Edited 11 Years Ago by asmasm
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
asmasm (13/08/2014)
Shouldn't you be copying the internal surface of the original manifold and not the external surface?


No...because the OEM manifold was meant primarily to reduce sound and maximize economy. 
asmasm
asmasm
Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)
Group: Forum Members
Posts: 15, Visits: 189
Edit:
Never mind, I see you are only doing half the intake in carbon and leaving the OEM runner dimensions.
Edited 11 Years Ago by asmasm
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search