Group: Forum Members
Posts: 468,
Visits: 2.7K
|
I've had things like this in the past. They do fill with lacquer and it looks OK but you do get a ripple in certain lights. If you ladle on the laquer and then flat it back you can get it properly smooth. I go down to about 360 and then recoat the lacquer. Anything smoother than 360 is wasting your time IMO.
|