How important is it to completely even out the part when sanding? I have a stubborn part that has a hard time leveling out, and after multiple sands and epoxy layers, it's not sticking well and letting me sand it level. Will adding clear coat cover this? or will it show through?

You can see some of the low spots in this picture:

http://www.talkcomposites.com/Uploads/Images/b04fa824-7194-43c6-b0a2-9eb.jpeg