hi newbie here!

         in case the lantor soric is not available in my area can i use coremat for vacuum infusion i'm planning to do CF hood with 200 grms cf 2/2 twill weave and 1mm coremat 400 grms wooven fabric.

Thanks
Reply
paul69401
paul69401
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 111
thanks for the reply sir hanaldo its help me a lotSmile