hi newbie here!
in case the lantor soric is not available in my area can i use coremat for vacuum infusion i'm planning to do CF hood with 200 grms cf 2/2 twill weave and 1mm coremat 400 grms wooven fabric.
Thanks
By paul69401
-
7/26/2014 8:04:23 AM
thanks for the reply sir hanaldo its help me a lot